MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for 3000 Series Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 3000 Series Aluminum Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "3000 Series Aluminum Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.0208 - 2.75 g/cc0.000752 - 0.0994 lb/in³Average value: 2.56 g/cc Grade Count:83
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 28.0 - 79.028.0 - 79.0Average value: 52.9 Grade Count:22
Hardness, Knoop 67.0 - 10267.0 - 102Average value: 86.1 Grade Count:11
Hardness, Vickers 29.0 - 89.029.0 - 89.0Average value: 71.7 Grade Count:9
Tensile Strength, Ultimate 90.0 - 295 MPa13100 - 42800 psiAverage value: 181 MPa Grade Count:44
Tensile Strength, Yield 29.0 - 285 MPa4210 - 41300 psiAverage value: 131 MPa Grade Count:44
Elongation at Break 1.00 - 40.0 %1.00 - 40.0 %Average value: 11.6 % Grade Count:44
Modulus of Elasticity 68.9 - 71.0 GPa9990 - 10300 ksiAverage value: 69.1 GPa Grade Count:44
Compressive Yield Strength 0.552 - 4.60 MPa80.0 - 667 psiAverage value: 2.05 MPa Grade Count:11
Compressive Modulus 0.110 - 1.02 GPa16.0 - 148 ksiAverage value: 0.460 GPa Grade Count:11
Notched Tensile Strength 110 - 303 MPa16000 - 43900 psiAverage value: 200 MPa Grade Count:5
Ultimate Bearing Strength 207 - 552 MPa30000 - 80100 psiAverage value: 339 MPa Grade Count:8
Bearing Yield Strength 83.0 - 345 MPa12000 - 50000 psiAverage value: 207 MPa Grade Count:8
Poissons Ratio 0.330 - 0.3500.330 - 0.350Average value: 0.338 Grade Count:30
Fatigue Strength 48.3 - 110 MPa7000 - 16000 psiAverage value: 82.7 MPa Grade Count:10
Machinability 10.0 - 50.0 %10.0 - 50.0 %Average value: 28.3 % Grade Count:12
Shear Modulus 0.0483 - 26.7 GPa7.00 - 3870 ksiAverage value: 14.6 GPa Grade Count:41
Shear Strength 0.310 - 180 MPa45.0 - 26100 psiAverage value: 71.2 MPa Grade Count:49
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000349 - 0.00000590 ohm-cm0.00000349 - 0.00000590 ohm-cmAverage value: 0.00000413 ohm-cm Grade Count:30
Magnetic Susceptibility 7.00e-7 - 8.00e-77.00e-7 - 8.00e-7Average value: 7.71e-7 Grade Count:17
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.5 - 25.5 µm/m-°C11.9 - 14.2 µin/in-°FAverage value: 23.7 µm/m-°C Grade Count:33
Specific Heat Capacity 0.880 - 0.897 J/g-°C0.210 - 0.214 BTU/lb-°FAverage value: 0.893 J/g-°C Grade Count:28
Thermal Conductivity 154 - 193 W/m-K1070 - 1340 BTU-in/hr-ft²-°FAverage value: 166 W/m-K Grade Count:28
Melting Point 629 - 655 °C1170 - 1210 °FAverage value: 645 °C Grade Count:26
Solidus 629 - 643 °C1170 - 1190 °FAverage value: 635 °C Grade Count:26
Liquidus 654 - 655 °C1210 - 1210 °FAverage value: 655 °C Grade Count:26
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 343 - 413 °C650 - 775 °FAverage value: 389 °C Grade Count:35
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 94.3 - 99.8 %94.3 - 99.8 %Average value: 97.1 % Grade Count:80
Chromium, Cr 0.0500 - 0.400 %0.0500 - 0.400 %Average value: 0.154 % Grade Count:40
Copper, Cu 0.0300 - 0.900 %0.0300 - 0.900 %Average value: 0.235 % Grade Count:80
Iron, Fe 0.0500 - 1.00 %0.0500 - 1.00 %Average value: 0.665 % Grade Count:78
Magnesium, Mg 0.0500 - 1.50 %0.0500 - 1.50 %Average value: 0.528 % Grade Count:62
Manganese, Mn 0.0500 - 1.80 %0.0500 - 1.80 %Average value: 0.903 % Grade Count:80
Nickel, Ni 0.0500 - 0.100 %0.0500 - 0.100 %Average value: 0.0600 % Grade Count:5
Silicon, Si 0.0800 - 1.80 %0.0800 - 1.80 %Average value: 0.506 % Grade Count:78
Titanium, Ti 0.0300 - 0.350 %0.0300 - 0.350 %Average value: 0.101 % Grade Count:46
Vanadium, V 0.0500 %0.0500 %Average value: 0.0500 % Grade Count:3
Zinc, Zn 0.0500 - 1.30 %0.0500 - 1.30 %Average value: 0.278 % Grade Count:80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for 5000 Series Aluminum Alloy
Overview of materials for 6000 Series Aluminum Alloy
Overview of materials for 2000 Series Aluminum Alloy
Overview of materials for 4000 Series Aluminum Alloy
Overview of materials for 1000 Series Aluminum

M01042 / 81684

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.