Purell GB7250 is an HDPE material which exhibits good flowability and high rigidity behaviors. Exceptional organoleptic properties and a good balance of stiffness, toughness and processability make Purell GB7250 the choice of customers for the production of closures for still mineral water and many other types of food and non-food caps and closures as well as tube shoulders. Applications: Caps & Closures, Caps & Closures (Healthcare), Collapsible Tubes, Healthcare Applications, Medical DevicesInformation provided by LyondellBasell. |