MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Purell PE GF 4750 High Density Polyethylene (HDPE), Blow Molding Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Purell PE GF4750 is a high density polyethylene with a good ESCR, containing antioxidants and delivered in pellet form. The grade is used for small blow moldings and tubes for packaging of consumer goods, surfactants, detergents as well as pharmaceuticals. Applications: Bottles and Vials, Caps & Closures, Caps & Closures (Healthcare), Collapsible Tubes, Collapsible Tubes (Healthcare), Diagnostic Applications, Healthcare Applications, Medical Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ISO 1183-1
Melt Flow  0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 1.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.5 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 30 g/10 min
@Load 21.6 kg,
Temperature 190 °C
30 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ISO 868
Ball Indentation Hardness 44.0 MPa6380 psiISO 2039-1
Tensile Strength, Yield 23.0 MPa3340 psiISO 527-1,-2
Elongation at Yield 10 %10 %ISO 527-1,-2
Tensile Modulus 1.00 GPa145 ksiISO 527-1,-2
Charpy Impact, Notched  0.550 J/cm²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
Type 1, Edgewise, Notch A; ISO 179
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 70.0 °C158 °FB50; ISO 306
 
Descriptive Properties
FNCT (hrs)65ISO 16770, 6.0 MPa, 2% Arkopal N100, 50°C
 9ISO 16770, 4.0 MPa, 2% Arkopal N100, 80°C
Processing MethodBlown Film, Extrusion Blow Molding, Injection Blow Molding, Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil PP1013H1 Polypropylene Homopolymer
Celanese Hostaform® MT24U01 POM, Medical Technology
LyondellBasell Purell GB 7250 High Density Polyethylene (HDPE), Injection Molded
Versalis Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene
Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin

PEQT8637 / 220271

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.