MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Shin-Etsu Silicones X-65-130U Electrically Conductive Silicone Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: ShinEtsu X65130 U is a black semiconductive silicone compound designed to give very low volume resistivity for molding and extruding.

Product Features:

  • Good processability.
  • Lower than average volume resistivity.
Typical Applications:
  • EMI gaskets.
  • Key pads.

Information Provided by Shin-Etsu Silicones of America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.28 g/cc1.28 g/ccDCBP Cure
 1.28 g/cc1.28 g/ccDBPH Cure
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070DCBP Cure
 7171DBPH Cure
Tensile Strength at Break 4.59 MPa665 psiDBPH Cure
 4.79 MPa695 psiDCBP Cure
Elongation at Break 130 %130 %DCBP Cure
 130 %130 %DBPH Cure
Tear Strength 12.3 kN/m70.0 pliDie B; DCBP Cure
 13.1 kN/m75.0 pliDie B; DBPH Cure
Compression Set 20 %
@Temperature 180 °C,
Time 79200 sec
20 %
@Temperature 356 °F,
Time 22.0 hour
DCBP Cure
 
Descriptive Properties
Cure AgentDBPH
 DBPH-50
Cure TypePress Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Wacker Elastosil® LR 3141/50 A/B Liquid Silicone Rubber
Overview of materials for Liquid Silicone Rubber
Abatron L060421-1 Heat-Resistant Non-Flammable Silicone Rubber
Rogers Arlon CP-375CR Silicone Rubber

PSHIN273 / 177784

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.