MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elix Polymers Elix™ DP M116GF ABS Polymer
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled

Material Notes: High flow GF reinforced ABS (16%). Excellent balance of impact strength, rigidity, and flowabiltiy. Good dimensions stability. High rigidity, Physical form: white to slightly yellowish pellets. Main Applications: Household appliances, Housings (phone, computer, printer). Automotive interior, Automotive exterior, Toys, Cosmetics packaging, Extruded sheets, Medical devices, Electroplating, Pipes, Covers, Smart cards.

Property data measured at 23°C and 50% RH.

Information provided by Elix Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183-1
Melt Flow 15 g/10 min
@Load 10.0 kg,
Temperature 220 °C
15 g/10 min
@Load 22.0 lb,
Temperature 428 °F
cm³/10 min MVR; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 125 MPa18100 psiISO 2039-1
Tensile Strength, Yield 95.0 MPa13800 psi50 mm/min; ISO 527-1,2
Tensile Modulus 5.75 GPa834 ksi1mm/min.; ISO 527-1,2
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 106 °C223 °F50N 50°C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °Finjection molding; ISO 294
Mold Temperature 70.0 °C158 °Finjection molding; ISO 294
Injection Velocity 540 mm/sec21.3 in/secinjection molding; ISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elix Polymers Elix™ HH 3105 ABS Polymer
E-Polymers TEKAMID® TA250GFR , Flame Retardant, 25% Glass Fiber Reinforced PA66, DAM
Ravago Manufacturing Americas Hylac GP74G20 ABS
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose
LG Chemical HF380XC ABS, High Flow, High Surface Gloss

PELIX910 / 192505

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.