MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elix Polymers Elix™ HH 3105 ABS Polymer
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: High heat resistance ABS. Excellent balance of impact strength and flowability, super low emission grade, lower mould deposits in injection molding processing applications, better dimensional under heat. Physical form: white to slightly yellowish pellets. Main Applications: Household

Property data measured at 23°C and 50% RH. appliances, Housings (phone, computer, printer). Automotive interior, Automotive exterior, Toys, Cosmetics packaging, Extruded sheets, Medical devices, Electroplating, Pipes, Covers, Smart cards.

Information provided by Elix Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³ISO 1183-1
Linear Mold Shrinkage, Flow 0.0060 - 0.0070 cm/cm
@Thickness 2.00 mm
0.0060 - 0.0070 in/in
@Thickness 0.0787 in
60 X 60 mm; ISO-294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.0070 cm/cm
@Thickness 2.00 mm
0.0060 - 0.0070 in/in
@Thickness 0.0787 in
60 X 60 mm; ISO-294-4
Melt Flow 16 g/10 min
@Load 10.0 kg,
Temperature 220 °C
16 g/10 min
@Load 22.0 lb,
Temperature 428 °F
cm³/10 min MVR; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 95.0 MPa13800 psiISO 2039-1
Tensile Strength, Yield 42.0 MPa6090 psi50 mm/min; ISO 527-1,2
Elongation at Break >= 32 %>= 32 %50 mm/min; ISO 527-1,2
Tensile Modulus 2.15 GPa312 ksi1mm/min.; ISO 527-1,2
Flexural Strength 66.0 MPa9570 psi2mm/min; ISO 178
Flexural Modulus 2.26 GPa328 ksi2mm/min; ISO 178
Izod Impact, Notched (ISO)  11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 18.0 kJ/m²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Charpy Impact Unnotched 1.90 J/cm²
@Temperature 23.0 °C
9.04 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 99.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
55.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,2
Deflection Temperature at 0.46 MPa (66 psi) 104 °C219 °FISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C210 °FISO 75-1,2
Vicat Softening Point 103 °C217 °FB50, 50°C/h; ISO 306
 105 °C221 °FB120, 120°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Flammability Test >= 50
@Thickness 2.00 mm
>= 50
@Thickness 0.0787 in
US-FMVSS , mm/min; ISO 3795
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °Finjection molding; ISO 294
Mold Temperature 70.0 °C158 °Finjection molding; ISO 294
Injection Velocity 240 mm/sec9.45 in/secinjection molding; ISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elix Polymers Elix™ DP M116GF ABS Polymer
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat
Omni Plastics OmniTech™ ABS 24 HH ABS
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade
INEOS Styrolution Novodur® HH-112 ABS

PELIX913 / 192508

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.