MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eurofoam Polycell PE 30 Polyethylene Foam
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Closed-cell polyethylene foam. Extruded reticulated pieces. Excellent physical properties both for active and static uses. Adjustable softness, elasticity, thermal deformation, shock absorbing. Used as thermal insulation. Feastures minimal water absorption, low water-vapour permeability, resistance to atmospheric agents, non-polluting, chemically inert.

Information provided by Eurofoam s.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0200 - 0.0400 g/ccISO 845-88
Water Absorption <= 5.0 %ASTM D 1056
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 45 - 55ASTM D 2240
Tensile Strength 0.200 MPaASTM D 412
Elongation at Break >= 200 %ASTM D 412
Tear Strength 0.120 kN/mASTM D 624
Compression Set 15 %
@Strain 25 %
ASTM D 395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °CASTM D 3575
Minimum Service Temperature, Air -30.0 °CASTM D 3575
Shrinkage <= 5.0 %
@Temperature 70.0 °C,
Time 605000 sec
Linear; ASTM D 1204
 
Descriptive Properties
Cellular StructureClosed
ColorGrey, White
Declaration of Heavy Metal AbsenceConformRoHS2002/95/EC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CoreLite PET® Closed-Cell Polyester Foam
Dow STRANDFOAM™ EA 1000 Polypropylene Foam
Eurofoam Polycell PLZ 45 Polyethylene Foam
INEOS Styrolution PS-168M Polystyrene
Polimeros Mexicanos Rotofoam® Plus 93050 Medium Density Polyethylene, Foam Grade

PEUROF926 / 157189

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.