MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution PS-168M Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Description: Polystyrene 168M is a high heat, high molecular weight general purpose polystyrene with excellent clarity and high stiffness. Due to its high melt strength and high stiffness. PS-168M is also an excellent choice for food packaging made form extruded foam sheet and biaxially oriented sheet. It offers high stiffness which is designed for extrusion/thermoforming applications, especially for food packaging.

Application: Include foamed meat and poultry trays, dinnerware, egg cartons, salad and fruit containers and fast food packaging.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.01143 cm/cm0.01143 in/inASTM D955
Melt Flow 1.5 g/10 min1.5 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7878ASTM D785
Tensile Strength at Break 52.0 MPa7540 psiASTM D638
Flexural Modulus 3.31 GPa480 ksiASTM D790
Izod Impact, Notched 0.160 J/cm0.300 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C201 °FASTM D648
Vicat Softening Point 109 °C
@Load 1.02 kg
228 °F
@Load 2.25 lb
Rate 120°C/hr; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Zone 1 138 - 177 °C280 - 351 °F
Zone 2 149 - 193 °C300 - 379 °F
Zone 3 193 - 216 °C379 - 421 °F
Zone 4 216 - 238 °C421 - 460 °F
Melt Temperature 210 - 238 °C410 - 460 °F
Drying Temperature 71.0 °C160 °F
Dry Time 2 - 4 hour2 - 4 hour
 
Descriptive Properties
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurofoam Polycell PE 30 Polyethylene Foam
Dow STRANDFOAM™ EA 1000 Polypropylene Foam
BASF Ultramid® 8253 HS PA6 (Dry)
Total PSC 1960N Crystal Polystyrene
American Polymers API 375 Polystyrene

PBASG0571 / 132204

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.