MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Unifrax Fiberfrax® Duraback® Ceramic Fiber Insulator
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax Duraback blanket is a strong, lightweight, flexible needled blanket intended for use as a cost-effective back-up insulation in Fiberwall® furnace linings. It is recommended for use up to 982°C (1800°F).

Duraback blanket can be installed up to four times faster than common block-type back-up insulation.

    Typical Applications
  • Back-up for Fiberwall® lining systems
  • Filler for insulating pads
  • Expansion joint material

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.73 g/cc2.73 g/cc
Density 0.0641 g/cc0.00231 lb/in³
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.13 J/g-°C
@Temperature 1093 °C
0.270 BTU/lb-°F
@Temperature 1999 °F
Melting Point 1648 °C2998 °F
Maximum Service Temperature, Air 982 °C1800 °FRecommended Operating Temperature
 
Component Elements PropertiesMetricEnglishComments
Al2O3 31 - 35 %31 - 35 %
CaO <= 7.5 %<= 7.5 %
Fe2O3 1.3 %1.3 %
MgO 0.50 %0.50 %
SiO2 50 - 54 %50 - 54 %
TiO2 1.7 %1.7 %
ZrO2 5.0 %5.0 %
 
Descriptive Properties
Average Fiber Diameter (microns)2-4
ColorWhite
Fiber Diameter (microns)2-4
Temperature Grade (°C)982

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceraform 100 Ceramic Fiber
Unifrax Fiberfrax® 110 Ceramic Fiber Paper
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator

CUNIF018 / 97790

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.