MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Unifrax Fiberfrax® 110 Ceramic Fiber Paper
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: 110 paper is a clay-filled, sheeted ceramic fiber paper which is denser and more rigid than other standard grade products. The rigidity is maintained even after burnout of the organic bonding agents. The good dielectric strength, compression resistance, and die cutting characteristics of 110 paper are advantageous in many high-temperature gasketing applications.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.288 g/cc0.0104 lb/in³
Loss On Ignition 8.5 %8.5 %including binder
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 1.71 MPa248 psiAs manufactured
Tensile Strength, Yield 1.01 MPa147 psiAs manufactured
Compressive Strength 0.0276 MPa4.00 psi10% deformation
 0.179 MPa26.0 psi25% deformation
 1.15 MPa167 psi50% deformation
 
Thermal PropertiesMetricEnglishComments
Melting Point 1538 °C2800 °F
Maximum Service Temperature, Air 1040 °C1900 °FRecommended Operating Temperature
 
Component Elements PropertiesMetricEnglishComments
Al2O3 45 - 50 %45 - 50 %
Fe2O3 <= 1.1 %<= 1.1 %
SiO2 40 - 44 %40 - 44 %
 
Descriptive Properties
ColorTan
Na2O3 (%)<1.5
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Morgan Advanced Ceramics Ceraform 100 Ceramic Fiber
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Unifrax Fiberfrax® Duraback® Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator

CUNIF003 / 97775

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.