MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical properties and high tear strength.

Performance Features:

  • High production rates
  • Good melt flow
  • Softener-free
  • High oil resistance
  • Dynamically highly loadable
Applications: For the production of profiles, spiral hoses, jackets for high pressure hoses

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccInjection molded
Linear Mold Shrinkage 0.0090 in/inInjection molded; ASTM D955
Melt Index of Compound 25 g/10 min
@Load 21.6 kg,
Temperature 190 °C
MVR, [cm3/10 min]
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80Injection molded parts; ASTM D2240
Hardness, Shore D 30Injection molded parts; ASTM D2240
Tensile Strength at Break 50.0 MPaInjection molded parts; DIN 53504
Elongation at Break 700 %Injection molded parts; DIN 53504
100% Modulus 0.00440 GPa
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 0.00800 GPa
@Strain 300 %
Injection molded parts; DIN 53504
Tear Strength 342 pliInjection molded parts; DIN 53515
Abrasion 25mm3, Injection molded; ISO 4649
Compression Set 21 %
@Temperature 22.8 °C,
Time 86400 sec
Injection molded; ASTM D395
 36 %
@Temperature 70.0 °C,
Time 86400 sec
Injection molded; ASTM D395
 
Processing PropertiesOriginal ValueComments
Feed Temperature 25.0 - 40.0 °CExtrusion
Middle Barrel Temperature 165 - 190 °CExtrusion
Nozzle Temperature 170 - 200 °CExtrusion
 180 - 200 °CInjection
Adapter Temperature 175 - 195 °CExtrusion
Die Temperature 175 - 200 °CExtrusion
Melt Temperature 170 - 195 °CInjection
Mold Temperature 68.0 - 158 °FInjection
 
Descriptive Properties
Heating Zone175-195°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sunoco D115A Polypropylene Homopolymer
Sunoco CP360H Polypropylene Homopolymer
E-Polymers EFLEX® M400 PP Homopolymer
Avient Maxxam™ PPH-20C UV Natural Polypropylene Homopolymer (PP Homopolymer)

PHUQ090 / 159463

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.