MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 78 E 4506 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical properties and high tear strength.

Performance Features:

  • High production rates
  • Good melt flow
  • Softener-free
  • High oil resistance
  • Dynamically highly loadable
Applications: For the production of profiles, spiral hoses, jackets for high pressure hoses

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³Injection molded
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inInjection molded; ASTM D955
Melt Index of Compound 25 g/10 min
@Load 21.6 kg,
Temperature 190 °C
25 g/10 min
@Load 47.6 lb,
Temperature 374 °F
MVR, [cm3/10 min]
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080Injection molded parts; ASTM D2240
Hardness, Shore D 3030Injection molded parts; ASTM D2240
Tensile Strength at Break 50.0 MPa7250 psiInjection molded parts; DIN 53504
Elongation at Break 700 %700 %Injection molded parts; DIN 53504
100% Modulus 4.40 MPa
@Strain 100 %
638 psi
@Strain 100 %
Injection molded parts; DIN 53504
300% Modulus 8.00 MPa
@Strain 300 %
1160 psi
@Strain 300 %
Injection molded parts; DIN 53504
Tear Strength 60.0 kN/m342 pliInjection molded parts; DIN 53515
Abrasion 2525mm3, Injection molded; ISO 4649
Compression Set  21 %
@Temperature 22.8 °C,
Time 86400 sec
21 %
@Temperature 73.0 °F,
Time 24.0 hour
Injection molded; ASTM D395
 36 %
@Temperature 70.0 °C,
Time 86400 sec
36 %
@Temperature 158 °F,
Time 24.0 hour
Injection molded; ASTM D395
 
Processing PropertiesMetricEnglishComments
Feed Temperature 25.0 - 40.0 °C77.0 - 104 °FExtrusion
Middle Barrel Temperature 165 - 190 °C329 - 374 °FExtrusion
Nozzle Temperature 170 - 200 °C338 - 392 °FExtrusion
 180 - 200 °C356 - 392 °FInjection
Adapter Temperature 175 - 195 °C347 - 383 °FExtrusion
Die Temperature 175 - 200 °C347 - 392 °FExtrusion
Melt Temperature 170 - 195 °C338 - 383 °FInjection
Mold Temperature 20.0 - 70.0 °C68.0 - 158 °FInjection
 
Descriptive Properties
Heating Zone175-195°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sunoco D115A Polypropylene Homopolymer
Sunoco CP360H Polypropylene Homopolymer
E-Polymers EFLEX® M400 PP Homopolymer
Avient Maxxam™ PPH-20C UV Natural Polypropylene Homopolymer (PP Homopolymer)

PHUQ090 / 159463

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.