MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Nylon 6, Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.11 - 1.90 g/ccAverage value: 1.27 g/cc Grade Count:86
Filler Content 1.00 - 50.0 %Average value: 31.8 % Grade Count:20
Water Absorption 0.500 - 6.80 %Average value: 1.54 % Grade Count:17
Moisture Absorption at Equilibrium 0.800 - 3.32 %Average value: 1.94 % Grade Count:23
Water Absorption at Saturation 3.50 - 6.50 %Average value: 5.09 % Grade Count:11
Additive Loading 15.0 - 40.0 %Average value: 26.3 % Grade Count:4
Maximum Moisture Content 0.0200 - 0.150Average value: 0.118 Grade Count:4
 0.200 - 0.200
@Temperature 120 - 120 °C
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.000200 - 0.0110 cm/cmAverage value: 0.00332 cm/cm Grade Count:48
Linear Mold Shrinkage, Transverse 0.00100 - 0.0140 cm/cmAverage value: 0.00663 cm/cm Grade Count:26
Melt Flow 3.00 - 60.0 g/10 minAverage value: 25.0 g/10 min Grade Count:11
Ash 10.0 - 30.0 %
@Temperature 550 - 550 °C
Average value: 20.0 % Grade Count:2
 10.0 - 30.0 %
@Time 600 - 600 sec
Average value: 20.0 % Grade Count:2
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115 - 119Average value: 116 Grade Count:8
Ball Indentation Hardness 90.0 - 320 MPaAverage value: 219 MPa Grade Count:7
Tensile Strength, Ultimate 1.00 - 1910 MPaAverage value: 231 MPa Grade Count:79
Tensile Strength, Yield 138 - 221 MPaAverage value: 196 MPa Grade Count:8
Elongation at Break 1.00 - 20.0 %Average value: 3.31 % Grade Count:80
Modulus of Elasticity 3.50 - 135 GPaAverage value: 19.1 GPa Grade Count:71
Flexural Yield Strength 75.0 - 1040 MPaAverage value: 300 MPa Grade Count:61
Flexural Modulus 3.40 - 97.9 GPaAverage value: 17.0 GPa Grade Count:56
Izod Impact, Notched 0.255 - 2.67 J/cmAverage value: 1.12 J/cm Grade Count:26
Izod Impact, Unnotched 5.34 - 17.1 J/cmAverage value: 8.87 J/cm Grade Count:14
Izod Impact, Notched (ISO) 5.00 - 30.0 kJ/m²Average value: 14.5 kJ/m² Grade Count:15
 11.0 - 18.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 14.8 kJ/m² Grade Count:6
Izod Impact, Unnotched (ISO) 45.0 - 90.0 kJ/m²Average value: 71.3 kJ/m² Grade Count:8
 60.0 - 93.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 72.2 kJ/m² Grade Count:6
Charpy Impact Unnotched 2.20 J/cm² - NBAverage value: 6.02 J/cm² Grade Count:32
 4.00 - 6.51 J/cm²
@Temperature -30.0 - -20.0 °C
Average value: 5.01 J/cm² Grade Count:5
Charpy Impact, Notched 0.300 - 3.57 J/cm²Average value: 1.22 J/cm² Grade Count:42
 0.300 - 1.995 J/cm²
@Temperature -30.0 - -20.0 °C
Average value: 1.10 J/cm² Grade Count:5
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00500 - 1.00e+16 ohm-cmAverage value: 3.04e+14 ohm-cm Grade Count:37
Surface Resistance 0.190 - 1.00e+13 ohmAverage value: 5.03e+11 ohm Grade Count:36
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.00 - 80.0 µm/m-°CAverage value: 23.0 µm/m-°C Grade Count:16
CTE, linear, Transverse to Flow 3.00 - 60.0 µm/m-°CAverage value: 24.5 µm/m-°C Grade Count:4
Melting Point 200 - 315 °CAverage value: 228 °C Grade Count:41
Maximum Service Temperature, Air 100 - 260 °CAverage value: 154 °C Grade Count:10
Deflection Temperature at 0.46 MPa (66 psi) 190 - 280 °CAverage value: 217 °C Grade Count:24
Deflection Temperature at 1.8 MPa (264 psi) 170 - 282 °CAverage value: 210 °C Grade Count:49
Deflection Temperature at 8.0 MPa 100 - 240 °CAverage value: 148 °C Grade Count:6
Vicat Softening Point 165 - 255 °CAverage value: 204 °C Grade Count:17
Minimum Service Temperature, Air -60.0 °CAverage value: -60.0 °C Grade Count:5
Glass Transition Temp, Tg 5.00 - 74.2 °CAverage value: 50.4 °C Grade Count:7
Flammability, UL94 HB - V-0Grade Count:37
 
Processing PropertiesOriginal ValueComments
Processing Temperature 221 - 300 °CAverage value: 262 °C Grade Count:5
Nozzle Temperature 230 - 300 °CAverage value: 265 °C Grade Count:12
Melt Temperature 220 - 340 °CAverage value: 266 °C Grade Count:54
Mold Temperature 50.0 - 135 °CAverage value: 86.7 °C Grade Count:53
Injection Velocity 30.0 - 76.2 mm/secAverage value: 56.1 mm/sec Grade Count:5
Drying Temperature 73.9 - 120 °CAverage value: 87.1 °C Grade Count:51
Moisture Content 0.0500 - 0.200 %Average value: 0.147 % Grade Count:21
Dew Point -17.8 °CAverage value: -17.8 °C Grade Count:6
Injection Pressure 30.0 - 130 MPaAverage value: 88.2 MPa Grade Count:15
Cushion 0.635 cmAverage value: 0.635 cm Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Overview of materials for Nylon 6, Extruded
Overview of materials for Nylon 6, 50% Glass Fiber Filled
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade

O2441 / 77988

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.