MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Crosspolimeri FRAGOM PR/6 92 Flame Retardant Polyolefinic
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: FRAGOM: is the trade-mark of our flame retardant halogen free polyolefine thermoplastic compounds

FRAGOM PR/6 92: flame retardant polyolefine thermoplastic compound having high temperature index and good oxygen index, suitable for cable sheathing and insulation.

Certify: CEI 2011TM9, CEI 2022 II/III

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
Melt Flow 8.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
Storage Temperature 12.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 51ASTM D2240
Tensile Strength 11.48 MPaHydrocarbons resistance; ENI 018100
 14.0 MPaIEC 811
 11.2 MPa
@Temperature 70.0 °C,
Time 14400 sec
Oil resistance, SAE 20; IEC 811
 16.8 MPa
@Temperature 100 °C,
Time 605000 sec
Heat Ageing; IEC 811
Elongation at Break 180 %IEC 811
 189 %Hydrocarbons resistance; ENI 018100
 147.6 %
@Temperature 100 °C,
Time 605000 sec
Heat Ageing; IEC 811
 184.5 %
@Temperature 70.0 °C,
Time 14400 sec
Oil resistance, SAE 20; IEC 811
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmBS 6622
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 80.0 °C
@Time 14400 sec
30%, Penetration (K=0,6); IEC 811
Oxygen Index 37 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 120 °C
Zone 2 150 °C
Zone 3 160 °C
Zone 4 170 °C
Die Temperature 185 °C
Head Temperature 180 °C
 
Descriptive Properties
Corrosivity of gases evolved>4,3 pHIEC 754-2
Halogen Content< 0,3%IEC 754-1
Temperature Index Value>330°C21% O2, NES 715
Water absorption1,3 mg/cm²24 h at 100°C, IEC 60811

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCROS099 / 294183

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.