MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Crosspolimeri FRAGOM PR/6 92 Flame Retardant Polyolefinic
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: FRAGOM: is the trade-mark of our flame retardant halogen free polyolefine thermoplastic compounds

FRAGOM PR/6 92: flame retardant polyolefine thermoplastic compound having high temperature index and good oxygen index, suitable for cable sheathing and insulation.

Certify: CEI 2011TM9, CEI 2022 II/III

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccASTM D792
Melt Flow 8.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
8.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5151ASTM D2240
Tensile Strength 11.48 MPa1665 psiHydrocarbons resistance; ENI 018100
 14.0 MPa2030 psiIEC 811
 11.2 MPa
@Temperature 70.0 °C,
Time 14400 sec
1620 psi
@Temperature 158 °F,
Time 4.00 hour
Oil resistance, SAE 20; IEC 811
 16.8 MPa
@Temperature 100 °C,
Time 605000 sec
2440 psi
@Temperature 212 °F,
Time 168 hour
Heat Ageing; IEC 811
Elongation at Break 180 %180 %IEC 811
 189 %189 %Hydrocarbons resistance; ENI 018100
 147.6 %
@Temperature 100 °C,
Time 605000 sec
147.6 %
@Temperature 212 °F,
Time 168 hour
Heat Ageing; IEC 811
 184.5 %
@Temperature 70.0 °C,
Time 14400 sec
184.5 %
@Temperature 158 °F,
Time 4.00 hour
Oil resistance, SAE 20; IEC 811
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmBS 6622
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
30%, Penetration (K=0,6); IEC 811
Oxygen Index 37 %37 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Zone 1 120 °C248 °F
Zone 2 150 °C302 °F
Zone 3 160 °C320 °F
Zone 4 170 °C338 °F
Die Temperature 185 °C365 °F
Head Temperature 180 °C356 °F
 
Descriptive Properties
Corrosivity of gases evolved>4,3 pHIEC 754-2
Halogen Content< 0,3%IEC 754-1
Temperature Index Value>330°C21% O2, NES 715
Water absorption1,3 mg/cm²24 h at 100°C, IEC 60811

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS099 / 294183

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.