MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 2122 Metal Repair Aluminum Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: TRA-BOND 2122 is a versatile aluminum metal filled epoxy formulation developed for modern industrial casting, bonding and repair applications where a strong aluminum-like adhesive is required. This two-part 100% reactive epoxy system is easy to use as it bonds readily to aluminum and other non-ferrous and ferrous materials, to wood, ceramics, glass, concrete and to many plastics. It has low shrinkage, and cures fairly rapidly to a hard, tough solid. Fully cured TRA-BOND 2122 is strong and durable, and is further resistant to mild acids and alkalis, water, salts and salt solutions, petroleum solvents, lubricating oils, gasoline, jet fuels, alcohol and many other organic and inorganic compounds. It is a non-magnetic electrical insulator, does not rust, and can be drilled, sawed, cut and machined with regular metal working tools. TYPICAL REPAIR APPLICATIONS: molds, dies, fixtures, plumbing, automotive castings, aircraft, marine, salvage, ships, jigs, tool repair, small part manufacturing.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccMixed
Solids Content 100 %100 %Reactive Solids Content
Viscosity 60000 cP
@Temperature 25.0 °C
60000 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8686
Adhesive Bond Strength 9.65 MPa1400 psiLap shear, alum to alum, 24 hrs @ 25°C
 23.4 MPa3400 psiLap shear, alum to alum, 4 hrs @ 65°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cm
Dielectric Constant 8.5
@Frequency 1000 Hz
8.5
@Frequency 1000 Hz
Dielectric Strength 3.94 kV/mm100 kV/in
Dissipation Factor 0.10
@Frequency 1000 Hz
0.10
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C
@Temperature 20.0 °C
27.8 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 135 °C275 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Shrinkage 0.15 %0.15 %
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 65.0 °C
4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 20 min20 min
 
Descriptive Properties
Color Aluminum
Mix Ratio, parts by weight100/18Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC019 / 70947

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.