MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QSil 555 Addition Cure Potting Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QSil 555 is a 100% silicone semi-thixotropic compound designed for potting and encapsulation applications.

Key Features:

  • 100% solids - no solvents
  • Long pot life
  • Semi-thixotropic
  • Heat cure required

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/ccUncatalyzed, QSil 555B
 1.48 g/ccUncatalyzed, QSil 555A
Viscosity 3000 cPUncatalyzed, QSil 555B
 80000 cPUncatalyzed, QSil 555A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50Cure 15 minutes at 150°C
Tensile Strength 450 psiCure 15 minutes at 150°C
Elongation at Break 100 %Cure 15 minutes at 150°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.51e+15 ohm-cm
Dielectric Constant 3.27
@Frequency 1000 Hz
Dissipation Factor 0.0090
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Temperature 150 °C
 45.0 min
@Temperature 120 °C
 60.0 min
@Temperature 100 °C
Gel Time >= 4320 minCatalyzed
 
Descriptive Properties
ColorClearUncatalyzed, QSil 555A
 ClearUncatalyzed, QSil 555B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Stratasys® FLX95050-DM Rubber-Like Digital Material
Momentive Performance Materials RTV8111 Silicone Rubber Compounds for Potting, Encapsulating and Sealing
Dow JCR 6140
Overview of materials for Liquid Silicone Rubber
Northstar Polymers MPP-A50A High Performance Polyether

PACC2096 / 199484

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.