MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow JCR 6140
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Former Dow Corning product.

Information provided by Dow Corning

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc
@Temperature 25.0 °C
1.00 g/cc
@Temperature 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040
Tensile Strength, Ultimate 2.500 MPa362.6 psi
Elongation at Break 110 %110 %
Modulus of Elasticity 0.00100 GPa0.145 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.10e+14 ohm-cm2.10e+14 ohm-cm
Dielectric Constant 2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.3991.399
 1.4061.406
 1.397
@Wavelength 1554 nm
1.397
@Wavelength 1554 nm
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Appearanceclear
Mix Ratio (X:1)100Base to Catalyst ETN

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV8111 Silicone Rubber Compounds for Potting, Encapsulating and Sealing
Master Bond MasterSil 922-LO Silicone
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
Stratasys® FLX95050-DM Rubber-Like Digital Material
Overview of materials for Liquid Silicone Rubber

PDOWCO362 / 106063

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.