MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plaskolite West Optix® CA-927 HF Clear Impact Modified Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: Impact modified acrylic resin, injection molding grade

Applications: A high flow, impact-modified acrylic resin for injection molding. This resin offers impact strengths up to seven times those of general-purpose acrylic resins and, at the same time, a high melt flow rate.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccASTM D792
Melt Flow 12 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 49.6 MPaASTM D638
Elongation at Break 25 %ASTM D638
Modulus of Elasticity 2.38 GPaASTM D638
Flexural Strength 48.3 MPaASTM D790
Izod Impact, Notched 0.430 J/cmASTM D256
Gardner Impact 28.0 in-lbFalling Weight; ASTM D3029GB
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °CASTM D648
Vicat Softening Point 108 °CRate A, ASTM D1525
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plaskolite West Optix® CA-927 G HF Clear Impact Modified Acrylic Resin
Plaskolite West Optix® CA-927 G Clear Impact Modified Acrylic Resin
Plaskolite West Optix® CA-86 Clear General Purpose Acrylic Resin
Plaskolite West Optix® CA-945 Clear Impact Modified Acrylic Resin
Plaskolite West Optix® CA-1000 IG UC Clear High Impact Acrylic Resin

PCA220 / 27907

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.