MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Plaskolite West Optix® CA-1000 IG UC Clear High Impact Acrylic Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: High impact acrylic resin, injection molding and extrusion grade

Applications: A premium impact acrylic resin particularly suited for medical and food uses. This resin is suited for Gamma irradiation treatment. Meets FDA CFR-21 Sec 177.1010 for food use. Meets USP Plastic Class VI for medical use.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ASTM D792
Melt Flow 1.6 g/10 min1.6 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 40.0 MPa5800 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Modulus of Elasticity 1.38 GPa200 ksiASTM D638
Flexural Strength 46.9 MPa6800 psiASTM D790
Izod Impact, Notched 0.640 J/cm1.20 ft-lb/inASTM D256
Gardner Impact 6.10 J4.50 ft-lbFalling weight impact per ASTM D3029 GB
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C172 °FASTM D648
Vicat Softening Point 100 °C212 °FRate A, ASTM D1525
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90.8 %90.8 %ASTM D1003
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin
Plaskolite West Optix® CA-927 G HF Clear Impact Modified Acrylic Resin
Plaskolite West Optix® CA-927 HF Clear Impact Modified Acrylic Resin
Plaskolite West Optix® CA-86 Clear General Purpose Acrylic Resin
Plaskolite West Optix® CA-927 G Clear Impact Modified Acrylic Resin

PCA030 / 27899

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.