MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M 25A87 Co-Extruded Polyethylene Protective Tapes
Categories: Polymer; Adhesive

Material Notes: 3M™ Co-Extruded Polyethylene Protective Tape have a high-tack adhesive system to help provide temporary protection of many matte finished plastic laminate tops, cultured marble, textured plastics and metals form surface damage, such as scratching abrading, etc.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 3.00 milASTM D3652
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 0.8125 pliAdhesion to Steel; ASTM D3330
 
Descriptive Properties
Adhesive TypeAcrylic
AppearanceClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SPHERE ONE EXTENDOSPHERES™ XOL-150 Hollow Spheres
3M 2A25 Co-Extruded Multi-Polymer Protect Tapes
3M 25A88 Co-Extruded Polyethylene Protective Tapes
3M 25A29 Co-Extruded Polyethylene Protective Tapes
3M 25A26 Co-Extruded Polyethylene Protective Tapes

PMM34280 / 169027

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.