MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SPHERE ONE EXTENDOSPHERES™ XOL-150 Hollow Spheres
Categories: Ceramic; Other Engineering Material; Additive/Filler for Polymer

Material Notes: EXTENDOSPHERES™ XOL-150 are white aluminosilicate multicellular hollow spheres. The density of this product is 0.30 g/cc. In plastic and coating applications, EXTENDOSPHERES™ XOL-150 hollow spheres can significantly reduce composite density. This product is recommended for cultured marble, syntactic foams and other low-shear applications. EXTENDOSPHERES™ XOL-150 hollow spheres are surface-modified to insure better dispersion, bonding and strength features in adverse environments. On a volume basis, EXTENDOSPHERES™ XOL-150 offers excellent economics when compared to other additives.

Information provided by Sphere One Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.170 g/cc0.00614 lb/in³
Density 0.300 g/cc0.0108 lb/in³
Particle Size 35 µm35 µmAverage Mean
 10 - 150 µm10 - 150 µm
pH 7.07.0
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 0.689 MPa100 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1300 °C2370 °FDeformation temp
 
Descriptive Properties
ColorWhite
Physical FormFree-Flowing Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fibre Glast 180 Clear Gel Coat
Potters Industries Q-Cel® 5023
Potters Industries Q-Cel® 5028
Saxonburg Ceramics S-213 Cordierite
Akzo Nobel Expancel® 551 DE 40 d42 Dry expanded microspheres

CSPHERE02 / 2198

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.