MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 8622 Steel, heat treated, machined to 13.7 mm rounds, pseudocarburized, 150°C (300°F) temper
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 8000 Series Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel

Material Notes: Normalize 925°C (1700°F) in 32 mm rounds, machine to 13.7 mm rounds, pseudocarburize at 925°C (1700°F) for 8 hours, oil quench, 150°C (300°F) temper, tested in 12.8 mm rounds

Key Words: B.S. 805 A 20, UNS G86220, ASTM A322, ASTM A331, SAE J404, SAE J770, DIN 1.6543
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 429
Hardness, Knoop 461Converted from Brinell
Hardness, Rockwell B 105Converted from Brinell
Hardness, Rockwell C 46Converted from Brinell
Hardness, Vickers 455Converted from Brinell
Tensile Strength, Ultimate 1524 MPa
Tensile Strength, Yield 1149 MPa
@Strain 0.2 %
Elongation at Break 13.5 %in 50 mm
Modulus of Elasticity 205 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel.
Poissons Ratio 0.29Calculated
Machinability 65 %annealed and cold drawn. Based on AISI 1212 steel = 100%.
Shear Modulus 80.0 GPaTypical for steel.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000234 ohm-cmTypical steel
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.475 J/g-°CTypical steel
Thermal Conductivity 46.6 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.20 - 0.25 %
Chromium, Cr 0.40 - 0.60 %
Iron, Fe 96.925 - 98 %As remainder
Manganese, Mn 0.70 - 0.90 %
Molybdenum, Mo 0.15 - 0.25 %
Nickel, Ni 0.40 - 0.70 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.30 %
Sulfur, S <= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 205°C (400°F) temper, 25 mm (1 in.) round
AISI 8620H Steel, mock carburized, reheated and oil quenched, 150°C (300°F) temper, 13 mm (0.5 in.) round
AISI 8620H Steel, normalized, machined to 13.7 mm, pseudocarburized, reheated to 840°C, 150°C temper
AISI 8620H Steel, normalized, machined to 25 mm, pseudocarburized, oil quenched, 150°C temper
AISI 8622 Steel, heat treated, machined to 25 mm (1 in.) rounds, pseudocarburized, 150°C (300°F) temper

M862DK / 8368

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.