MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kennametal Stellite Nucalloy® 41 Nickel-Chromium-Boron Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Stood® 41 is a nickel-chromium-boron alloy. Stood 41 can be certified to meet MIL-N-24422 (ships) Composition A. Stood 41 derives its superior wear resistance from the presence of hard nickel borides - and to a lesser extent, chromium carbides - tightly held in a tough nickel-rich matrix. It is machinable with carbide tools and may be cast centrifugally or as a static casting.

Information provided by Deloro Stellite Inc. Deloro Stellite uses both the names Nucalloy® 41 and Stood® 41 for this alloy.

Product of former Deloro Stellite Inc.

Key Words: MIL-N-24422; Deloro Stellite Inc.
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 42 - 52
 
Component Elements PropertiesOriginal ValueComments
Boron, B 2.0 %
Carbon, C 0.50 %
Chromium, Cr 12.5 %
Iron, Fe 4.0 %
Nickel, Ni 76 %As Remainder
Other 1.0 %
Silicon, Si 4.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kennametal Stellite Nucalloy® 453 High-Silicon Nickel-Base Hardfacing Alloy
Kennametal Stellite Stellite® 6 PM with P/M Processing
Kennametal Stellite Stellite® 3 PM with P/M Processing
Kennametal Stellite Nucalloy® 488 High-Silicon Nickel-Base Hardfacing Alloy
Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy

NSNU4 / 19195

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.