MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Redwood Plastics Redco™ NEO CG60 Sheet Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Redco™ Neo™ CG60 is a polychloroprene blend with good resistance to abrasion and flex cracking. Formulated as an excellent general industrial material vs. cost, it is our most popular industrial grade. Polychloroprene (most commonly recognized by the tradename Neoprene™) is one of the most commonly used rubber materials. It offers the most balanced set of properties and the additional ability to resist oils. It is critical to confirm product specifications as there are a wide range of grades available in Redco™ Neoprene™.

Designation: CR, Chloroprene, Neoprene

Type: Commercial grade

Advantage:

  • Good resilience
  • Resistant to abrasion & flex cracking
  • Very good resistance to temperature, ozone and natural aging
  • Flame retardant
  • Good adhesion to metals and fabrics when properly applied
  • Good resistance to alkalis & acids

Limitation:

  • Does not resist majority of organic compounds including aromatic and oxygenated solvents
  • Limited properties at high and low temperature extremes.

Uses: Most common industrial grade of sheet rubber

Information provided by Redwood Plastics and Rubber

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 53 - 67ASTM D 2240
Tensile Strength 300 psiASTM D 412
Elongation at Break 300 %Ultimate; ASTM D412
Tear Strength 17.5 kN/mASTM D 624
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 82.0 °C
Minimum Service Temperature, Air -30.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREDW065 / 296631

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.