Redco™ Neo™ CG60 is a polychloroprene blend with good resistance to abrasion and flex cracking. Formulated as an excellent general industrial material vs. cost, it is our most popular industrial grade. Polychloroprene (most commonly recognized by the tradename Neoprene™) is one of the most commonly used rubber materials. It offers the most balanced set of properties and the additional ability to resist oils. It is critical to confirm product specifications as there are a wide range of grades available in Redco™ Neoprene™. Designation: CR, Chloroprene, Neoprene Type: Commercial grade Advantage: - Good resilience
- Resistant to abrasion & flex cracking
- Very good resistance to temperature, ozone and natural aging
- Flame retardant
- Good adhesion to metals and fabrics when properly applied
- Good resistance to alkalis & acids
Limitation: - Does not resist majority of organic compounds including aromatic and oxygenated solvents
- Limited properties at high and low temperature extremes.
Uses: Most common industrial grade of sheet rubber Information provided by Redwood Plastics and Rubber |