MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® E 2517 One-Component Epoxy Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast A 316-48 provides the following product characteristics:
  • One component
  • Low CTE
  • Low stress
  • Low viscosity
  • High temperature resistance

Cure: Heat cure

Filler Type: Oxide

Application: Encapsulation

Typical Applications: Heavy duty industrial and automotive applications

Loctite Stycast E 2517 epoxy encapsulant is formulated for use on bare chip protection in a variety of advanced packages where ease of flow and high thermal stability are required.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.725 g/cc
Water Absorption 0.080 %
@Time 86400 sec
Viscosity 22500 cPRheometer, Plate/Plate
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Na (Sodium) 10 ppmExtractable Ionic Content
Ionic Impurities - K (Potassium) 10 ppmExtractable Ionic Content
Ionic Impurities - Cl (Chloride) 10 ppmExtractable Ionic Content
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
Modulus of Elasticity 6.30 GPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.90e+15 ohm-cm
Dielectric Constant 4.1
@Frequency 1000 Hz
Dissipation Factor 0.0070
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.0 µm/m-°C
Thermal Conductivity 0.500 W/m-K
Maximum Service Temperature, Air 200 °C
Glass Transition Temp, Tg 220 °C
Shrinkage 1.1 %Cure Shrinkage
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 150 °C
Full Cure
 1.00 hour
@Temperature 120 °C
Precure
 2.00 hour
@Temperature 200 °C
Post Cure
Shelf Life 4.00 Month
@Temperature -40.0 - 0.000 °C
from date of manufacture
 
Descriptive Properties
AppearanceBlack Liquid
Ionic Impurities - NH4 (Ammonium) (ppm)10Extractable Ionic Content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHENK7942 / 255427

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.