MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Henkel Loctite® Stycast® E 2517 One-Component Epoxy Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast A 316-48 provides the following product characteristics:
  • One component
  • Low CTE
  • Low stress
  • Low viscosity
  • High temperature resistance

Cure: Heat cure

Filler Type: Oxide

Application: Encapsulation

Typical Applications: Heavy duty industrial and automotive applications

Loctite Stycast E 2517 epoxy encapsulant is formulated for use on bare chip protection in a variety of advanced packages where ease of flow and high thermal stability are required.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.725 g/cc0.06232 lb/in³
Water Absorption 0.080 %
@Time 86400 sec
0.080 %
@Time 24.0 hour
Viscosity 22500 cP22500 cPRheometer, Plate/Plate
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Na (Sodium) 10 ppm10 ppmExtractable Ionic Content
Ionic Impurities - K (Potassium) 10 ppm10 ppmExtractable Ionic Content
Ionic Impurities - Cl (Chloride) 10 ppm10 ppmExtractable Ionic Content
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Modulus of Elasticity 6.30 GPa914 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.90e+15 ohm-cm1.90e+15 ohm-cm
Dielectric Constant 4.1
@Frequency 1000 Hz
4.1
@Frequency 1000 Hz
Dissipation Factor 0.0070
@Frequency 1000 Hz
0.0070
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.0 µm/m-°C10.6 µin/in-°F
Thermal Conductivity 0.500 W/m-K3.47 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °F
Glass Transition Temp, Tg 220 °C428 °F
Shrinkage 1.1 %1.1 %Cure Shrinkage
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
Full Cure
 60.0 min
@Temperature 120 °C
1.00 hour
@Temperature 248 °F
Precure
 120 min
@Temperature 200 °C
2.00 hour
@Temperature 392 °F
Post Cure
Shelf Life 4.00 Month
@Temperature -40.0 - 0.000 °C
4.00 Month
@Temperature -40.0 - 32.0 °F
from date of manufacture
 
Descriptive Properties
AppearanceBlack Liquid
Ionic Impurities - NH4 (Ammonium) (ppm)10Extractable Ionic Content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHENK7942 / 255427

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.