MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CTC SunPro® SP 200 P 5000 Polypropylene Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB500, CPN 4492

Data provided by Composite Technologies (CTC).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/in24Hr; ISO 294 3/4
Linear Mold Shrinkage, Transverse 0.0153 cm/cm0.0153 in/in24Hr; ISO 294 3/4
Melt Flow 15 - 25 g/10 min15 - 25 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa2900 psiISO 527-1/2
Flexural Modulus 0.750 GPa109 ksi0.05 in/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²Low Temp; ISO 180/1eA
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 182 - 216 °C360 - 420 °F
Middle Barrel Temperature 193 - 227 °C380 - 440 °F
Front Barrel Temperature 204 - 216 °C400 - 420 °F
Nozzle Temperature 204 - 216 °C400 - 420 °F
Melt Temperature 204 - 227 °C400 - 440 °F
Mold Temperature 26.7 - 60.0 °C80.0 - 140 °F
Back Pressure 0.345 - 1.03 MPa50.0 - 150 psi
Clamp Pressure 27.6 - 34.5 MPa4000 - 5000 psi
 
Descriptive Properties
Boost Pressure (psi)500-1500
Hold Pressure50 - 75% of Boost
Screw SpeedMedium to Fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil PP8114E1 Impact Copolymer
ExxonMobil PP7414 Impact Copolymer
ExxonMobil PP7032E2 Impact Copolymer
DuPont Mobility and Materials Vespel® SP-211 Polyimide, 15% Graphite, 10% Teflon® Filled, Direct formed
ExxonMobil PP8224E1 Impact Copolymer

PCTC972 / 104745

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.