MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

DuPont Mobility and Materials Vespel® SP-211 Polyimide, 15% Graphite, 10% Teflon® Filled, Direct formed
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Has lowest coefficient of friction over wide range of operating conditions. Also, has lowest wear rate up to 300°F.

Applications: For low friction and wear applications in moderate temperature and PV environments. Bearings (bushings, washers, etc.).

Direct-formed properties were measured perpendicular to the forming direction unless specified. Machined properties are non-directional

Information provided by DuPont

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.46 g/cc1.46 g/ccASTM D792
Deformation 0.29 %0.29 %2000 psi; 122°F; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 51.7 MPa7500 psi73°F; ASTM D1708
 24.1 MPa
@Temperature 260 °C
3500 psi
@Temperature 500 °F
ASTM D1708
Elongation at Break 5.5 %5.5 %73°F; ASTM D1708
 5.3 %
@Temperature 260 °C
5.3 %
@Temperature 500 °F
ASTM D1708
Flexural Strength 34.5 MPa5000 psi500°F; ASTM D790
 68.9 MPa10000 psi73°F; ASTM D790
Flexural Modulus 1.38 GPa200 ksi500°F; ASTM D790
 2.76 GPa400 ksi73°F; ASTM D790
Compressive Strength 14.5 MPa2100 psi@1% strain; 73°F; ASTM D695
 27.6 MPa4000 psi@0.1% Offset; 73°F; ASTM D695
 75.8 MPa11000 psi@10% strain; 73°F; ASTM D695
Compressive Modulus 1.38 GPa200 ksi73°F; ASTM D695
Coefficient of Friction, Dynamic 0.0800.080PV-100,000. Steady State; Unlubricated in air.
 0.120.12PV-25,000. Steady State; Unlubricated in air.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 41.4 µm/m-°C
@Temperature 22.8 - 300 °C
23.0 µin/in-°F
@Temperature 73.0 - 572 °F
ASTM E-228
Thermal Conductivity 0.418 W/m-K2.90 BTU-in/hr-ft²-°F104°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® SP-211 Polyimide, 15% Graphite, 10% Teflon® Filled, Machined
Overview of materials for Polyetheretherketone, Unreinforced
Chemours Teflon® PTFE 7C Granular Molding Powder
Overview of materials for High Density Polyethylene (HDPE), Extruded
Delrin Delrin® 100 BK602 POM

PDU2007 / 32868

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.