MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Arkema Kynar Superflex® 2500-20 PVDF
Material Notes:

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 - 1.82 g/cc1.80 - 1.82 g/ccASTM D792
Density 1.79 g/cc0.0647 lb/in³ISO 1183
Water Absorption 0.030 %0.030 %Dry; Sim. to ISO 62
 <= 0.070 %<= 0.070 %ASTM D570
Viscosity 900000 - 1.60e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
900000 - 1.60e+6 cP
@Shear Rate 100 1/s,
Temperature 446 °F
Melt; ASTM D3835
Melt Flow  5.8 g/10 min
@Load 3.80 kg,
Temperature 232 °C
5.8 g/10 min
@Load 8.38 lb,
Temperature 450 °F
cm³/10 min Volumetric Rate; ISO 1133
 1.0 - 15 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.0 - 15 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50 - 5750 - 57ASTM D2240
Tensile Strength at Break 13.8 - 31.0 MPa2000 - 4500 psiASTM D638
Tensile Strength, Yield 15.0 MPa2180 psiDry; ISO 527-1/-2
 11.7 - 19.3 MPa1700 - 2800 psiASTM D638
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 500 - 800 %500 - 800 %ASTM D638
Elongation at Yield 18 %18 %Dry; ISO 527-1/-2
 17 - 25 %17 - 25 %ASTM D638
Tensile Modulus 0.241 - 0.379 GPa35.0 - 55.0 ksiASTM D638
 0.350 GPa50.8 ksiDry; ISO 527-1/-2
Flexural Strength 10.3 - 17.2 MPa
@Strain 5.0 %
1490 - 2490 psi
@Strain 5.0 %
ASTM D790
Flexural Modulus 0.193 - 0.276 GPa28.0 - 40.0 ksiASTM D790
Compressive Strength 13.8 - 20.7 MPa2000 - 3000 psiASTM D695
Izod Impact, Notched NBNBASTM D256
Izod Impact, Unnotched NBNBASTM D256
Charpy Impact, Notched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eA
Coefficient of Friction, Dynamic 0.540.54vs. steel; ASTM D1894
Coefficient of Friction, Static 0.490.49vs. steel; ASTM D1894
Taber Abrasion, mg/1000 Cycles 28 - 3328 - 33CS 17 1000g:pad; ASTM-G195-13A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm65% R.H; ASTM D257
Surface Resistivity per Square 8.50e+11 - 9.20e+11 ohm8.50e+11 - 9.20e+11 ohmASTM D257
Dielectric Constant 4.5 - 13.5
@Frequency 1000 Hz
4.5 - 13.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 0.800 - 1.10 kV/mm20.3 - 27.9 kV/inASTM D149
 12.0 kV/mm305 kV/inDry; IEC 60243-1
Dissipation Factor 0.050 - 0.29
@Frequency 100000 Hz
0.050 - 0.29
@Frequency 100000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 153 - 194 µm/m-°C85.0 - 108 µin/in-°FASTM D696
Specific Heat Capacity 0.745 - 0.958 J/g-°C0.178 - 0.229 BTU/lb-°FDSC
Thermal Conductivity 0.144 - 0.180 W/m-K0.999 - 1.25 BTU-in/hr-ft²-°FASTM D433
Melting Point 117 - 125 °C243 - 257 °FASTM D3418
 122 °C252 °F10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 31.0 °C87.8 °FDry; ISO 75-1/-2
 26.7 - 37.8 °C80.1 - 100 °FASTM D648
Glass Transition Temp, Tg -43.3 - -40.0 °C-45.9 - -40.0 °FASTM D7028
 -40.0 °C-40.0 °F10°C/min; Dry; ISO 11357-1/-2
Decomposition Temperature 375 °C707 °F1% wt. loss, TGA, in air
 410 °C770 °F1% wt. loss, TGA, in nitrogen
Flammability, UL94  V-0
@Thickness 1.00 mm
V-0
@Thickness 0.0394 in
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Yellow Card Available; Dry; IEC 60695-11-10
Oxygen Index 42 %42 %ASTM D2863
 44 %44 %Dry; ISO 4589-1/-2
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.401.40sodium D line; ASTM D542
 
Descriptive Properties
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveNo
Processing MethodsCoating
 Injection Molding
 Sheet Extrusion
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Kynar® 720E PVDF
Arkema KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Arkema Kynar Flex® PPA 2200 PVDF
Arkema KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Arkema KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding

PARKF753 / 193545

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.