MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Arkema KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, fire resistance, abrasion resistance; low-smoke emission; high purity

Applications:

  • Chemical processing – production, storage and transfer of corrosive fluids
  • Electronics – protective sheathing, plenum and wiring insulation
  • Semi-conductor industry
  • Food stuff and Healthcare industries
  • Transportation – fuel line and pipe, thermoformed body components

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.75 - 1.77 g/cc1.75 - 1.77 g/ccASTM D792
Density 1.76 g/cc0.0636 lb/in³ISO 1183
Water Absorption <= 0.040 %<= 0.040 %ASTM D570
 0.040 %0.040 %Dry; Sim. to ISO 62
Viscosity 2.35e+6 - 2.95e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
2.35e+6 - 2.95e+6 cP
@Shear Rate 100 1/s,
Temperature 446 °F
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/inDry; ISO 294-4, 2577
 0.020 cm/cm0.020 in/in
Melt Flow  5.6 g/10 min
@Load 21.6 kg,
Temperature 230 °C
5.6 g/10 min
@Load 47.6 lb,
Temperature 446 °F
cm³/10 min Volumetric Rate; ISO 1133
 6.0 - 14 g/10 min
@Load 21.6 kg,
Temperature 230 °C
6.0 - 14 g/10 min
@Load 47.6 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75 - 8075 - 80ASTM D2240
Tensile Strength at Break 31.0 - 48.3 MPa4500 - 7010 psiASTM D638
Tensile Strength, Yield 42.0 MPa6090 psiDry; ISO 527-1/-2
 34.5 - 51.7 MPa5000 - 7500 psiASTM D638
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 50 - 250 %50 - 250 %ASTM D638
Elongation at Yield 10 - 15 %10 - 15 %ASTM D638
 13 %13 %Dry; ISO 527-1/-2
Tensile Modulus 1.03 - 1.38 GPa149 - 200 ksiASTM D638
 1.40 GPa203 ksiDry; ISO 527-1/-2
Flexural Strength 48.3 - 62.1 MPa
@Strain 5.0 %
7010 - 9010 psi
@Strain 5.0 %
ASTM D790
Flexural Modulus 1.38 - 1.79 GPa200 - 260 ksiASTM D790
Compressive Strength 55.2 - 68.9 MPa8010 - 9990 psiASTM D695
Izod Impact, Notched 0.961 - 2.14 J/cm1.80 - 4.01 ft-lb/inASTM D256
Izod Impact, Unnotched 8.01 - 21.4 J/cm15.0 - 40.1 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.170.17vs. steel; ASTM D1894
Coefficient of Friction, Static 0.230.23vs. steel; ASTM D1894
Taber Abrasion, mg/1000 Cycles 7.0 - 9.07.0 - 9.0CS 17 1000g:pad; ASTM-G195-13A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cm65% R.H; ASTM D257
 2.00e+14 ohm-cm2.00e+14 ohm-cmDry; IEC 60093
Surface Resistivity per Square 5.10e+11 - 5.30e+11 ohm5.10e+11 - 5.30e+11 ohmASTM D257
Dielectric Constant  6.7
@Frequency 1e+6 Hz
6.7
@Frequency 1e+6 Hz
Dry; IEC 60250
 4.5 - 9.5
@Frequency 1000 Hz
4.5 - 9.5
@Frequency 1000 Hz
ASTM D150
 9.0
@Frequency 100 Hz
9.0
@Frequency 100 Hz
Dry; IEC 60250
Dielectric Strength 1.60 kV/mm40.6 kV/inASTM D149
 63.0 kV/mm1600 kV/inDry; IEC 60243-1
Dissipation Factor  0.070
@Frequency 1e+6 Hz
0.070
@Frequency 1e+6 Hz
Dry; IEC 60250
 0.010 - 0.21
@Frequency 100000 Hz
0.010 - 0.21
@Frequency 100000 Hz
ASTM D150
 0.13
@Frequency 100 Hz
0.13
@Frequency 100 Hz
Dry; IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 - 126 µm/m-°C50.0 - 70.0 µin/in-°FASTM D696
CTE, linear, Parallel to Flow 114 µm/m-°C
@Temperature -40.0 - 100 °C
63.3 µin/in-°F
@Temperature -40.0 - 212 °F
ISO 11359-1/-2
Specific Heat Capacity 0.745 - 0.958 J/g-°C0.178 - 0.229 BTU/lb-°FDSC
Thermal Conductivity 0.170 - 0.190 W/m-K1.18 - 1.32 BTU-in/hr-ft²-°FASTM D433
 0.190 W/m-K1.32 BTU-in/hr-ft²-°FMelt
Melting Point 161 °C322 °F10°C/min; Dry; ISO 11357-1/-3
 155 - 172 °C311 - 342 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 112 - 140 °C234 - 284 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 - 90.0 °C176 - 194 °FASTM D648
 85.0 °C185 °FDry; ISO 75-1/-2
Glass Transition Temp, Tg -40.0 °C-40.0 °F10°C/min; Dry; ISO 11357-1/-2
 -40.6 - -38.3 °C-41.1 - -36.9 °FASTM D7028
Decomposition Temperature 375 °C707 °F1% wt. loss, TGA, in air
 410 °C770 °F1% wt. loss, TGA, in nitrogen
Flammability, UL94 V-0V-0IEC 60695-11-10
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
IEC 60695-11-10
Oxygen Index 43 %43 %Dry; ISO 4589-1/-2
 44 %44 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.421.42sodium D line; ASTM D542
 
Descriptive Properties
Form as DeliveredPellets
Moisture SensitiveNo
Processing MethodsOther Extrusion
 Profile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Kynar® 720E PVDF
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Arkema KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Arkema KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Arkema Kynar Superflex® 2500-20 PVDF

PARKG902 / 144527

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.