MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Celanese Celstran® TPU-GF30-01-US TPU, 30% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced

Material Notes: 30% long strand glass fiber reinforced thermoplastic polyurethane

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D792
Density 1.43 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.00050 - 0.0010 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0015 - 0.0025 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 180 MPa5mm/min; ISO 527-2/1A
 31300 psiASTM D638
Elongation at Break 2.75 %5mm/min; ISO 527-2/1A
 2.9 %ASTM D638
Tensile Modulus 8500 MPa50mm/min; ISO 527-2/1A
 1.41e+6 psiASTM D638
Flexural Strength 270 MPaISO 178
 39400 psiASTM D790
Flexural Modulus 7700 MPaISO 178
 1.13e+6 psiASTM D790
Izod Impact, Notched 8.20 ft-lb/inASTM D256
Charpy Impact, Notched 39.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °CISO 75-1, -2
 185 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 90.0 °Ccavity
 250 - 260 °Chot runner
Feed Temperature 20.0 - 50.0 °C
Zone 1 240 - 250 °C
Zone 2 245 - 255 °C
Zone 3 245 - 260 °C
Zone 4 245 - 260 °C
Die Temperature 245 - 260 °C
Melt Temperature 245 - 260 °C
Drying Temperature 80.0 °C
Dry Time 4.00 hour
Moisture Content <= 0.050 %
 
Descriptive Properties
Injection moldingYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether
3D Systems DuraForm® HST Fiber Filled Nylon for SLS Systems
BASF Ultramid® 8202 PA6 (Dry)

PHCQ254 / 178709

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.