MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Larton MDT16-02 PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.95 g/cc
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.0 MPa
@Temperature 23.0 °C
Elongation at Break 0.40 %
@Temperature 23.0 °C
Tensile Modulus 12000 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 6.00 kJ/m²
Charpy Impact, Notched 1.50 kJ/m²
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 - 310 °C
Mold Temperature 130 - 140 °C
Drying Temperature 130 - 150 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Wacker Belsil® RG 100 Crosspolymer
Trelleborg S550 Silicone Rubber
Schott ZERODUR® K20 Glass Ceramic
Omnia Plastica Omniamid PA 6 - Akulon 6 - Dry

PLATH9659 / 177355

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.