MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Belsil® RG 100 Crosspolymer
Categories: Fluid; Polymer

Material Notes: BELSIL® RG 100 elastomer gel is an organosiloxane polymer dispersed in cyclopentasiloxane. It is a semitransparent gel that functions as a thickener in formulations while delivering smooth applications. Under shear stress BELSIL® RG 100 thins and allows easy incorporation of cosmetic ingredients like pigments.

Special features: BELSIL® RG 100 is easy to distribute on skin and gives a nice, non-greasy, silky skin feel. Evaporation of the volatile silicones leave a non-tacky film which improves the water resistance of formulations.

Application: BELSIL® RG 100 is a non-emulsifying elastomer gel that is supplied as a 20% active solution in cyclopentasiloxane. It provides a substantive hydrophobic film, making it ideal for use in sun care formulations. In lipsticks and foundations, it improves transfer resistance. It also can add a cushiony feel to powder formulations. BELSIL® RG 100 makes cosmetics easier to apply by adding lubricity. It can be used to thicken the oil phase of emulsions or anhydrous cosmetic formulations.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³
Solids Content 20 %20 %
Viscosity 125000 cP125000 cPdynamic
 
Thermal PropertiesMetricEnglishComments
Flash Point 63.0 °C145 °FASTM D93
 
Descriptive Properties
Appearancecreamy, semitransparent
SolubilityAlcohol1-10%
 BELSIL® CM 040>10%
 BELSIL® DM 0.65>10%
 BELSIL® DM 1 Plus>10%
 BELSIL® DM 10insoluble
 BELSIL® PDM 20>10%
 C12-15 alkyl benzoatesinsoluble
 Caprylic/Capric Triglyceridesinsoluble
 Castor oilinsoluble
 Decyl oleateinsoluble
 Dicapryly Ether>10%
 Ethanol1-10%
 Ethyhexyl Stearate>10%
 Ethylhexyl Methoxycinnamateinsoluble
 Ethylhexyl Salicylateinsoluble
 Glycerol1-10%
 Isopropyl myristate>10%
 Lanolin oilinsoluble
 Mineral Oilinsoluble
 Oleyl oleateinsoluble
 PEG-7 Glyceryl Cocoateinsoluble
 Propylene glycol1-10%
 Waterinsoluble

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Crystat® ABS (anti-static)
Trelleborg S550 Silicone Rubber
Schott ZERODUR® K20 Glass Ceramic
LATI Larton MDT16-02 PPS
DuPont Mobility and Materials Sorona® FG3301 NC010 PTT

PWACK9040 / 204569

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.