MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-socket connectors, power switches), halogen- and antimony free.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %23°C; 50% RH
Water Absorption at Saturation 0.40 %DIN 53495/1L
Linear Mold Shrinkage, Flow 0.0044 cm/cm60x60x2 mm; ISO 294
Linear Mold Shrinkage, Transverse 0.0124 cm/cm60x60x2 mm; ISO 294
Melt Flow 22.95 g/10 min
@Load 2.16 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 110 MPa50 mm/min; ISO 527-2
Elongation at Break 2.3 %50mm/min; ISO 527-2
Modulus of Elasticity 9.80 GPaISO 527-2
Flexural Strength 180 MPaISO 178
Charpy Impact Unnotched 45.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmIEC 93
Surface Resistance >= 1.00e+16 ohmIEC 93
Dielectric Constant 3.6IEC 250
Dissipation Factor 0.0137IEC 250
Comparative Tracking Index 525 VTest solution A; IEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 - 110 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN 53752
Melting Point 220 - 225 °CDSC; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75-2
Flammability, UL94 V-0
@Thickness 0.800 mm
 V-0
@Thickness 1.60 mm
Glow Wire Test 960 °C
@Thickness 3.00 mm
IEC 695
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 280 °CInjection-molding
Mold Temperature 60.0 - 100 °C
 
Descriptive Properties
ColorNatural, Colored, Black and Special Colors
Commercial StatusEurope
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® FRee B 4450 G5 LS 25% Glass Filled PBT
BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT
Eurotec® Tecodur® PB70 GR15 NL TD 28 PBT 15% glass fiber reinforced, UL94 V0, impact modified, high CTI
BASF Ultradur® B 4330 G6 HR 30% Glass Filled PBT
Polyplastics Duranex® CTN7133 Polybutylene Terephthalate (PBT), Higher comparative tracking index, FR, GF filled

PBASG0113 / 131747

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.