MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Description: Is a PBT, injection-molding grade with 30% glass fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance, e.g. automotive connectors and housings for electronic units under the hood.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C; 50% RH
Water Absorption at Saturation 0.40 %0.40 %DIN 53495/1L
Viscosity Test 108 cm³/g1.08 dl/gViscosity number; ISO 1628
Linear Mold Shrinkage, Flow 0.0045 cm/cm0.0045 in/in60x60x2 mm; ISO 294
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/in60x60x2 mm; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 130 MPa18900 psi50 mm/min; ISO 527-2
Elongation at Break 3.3 %3.3 %50mm/min; ISO 527-2
Modulus of Elasticity 8.70 GPa1260 ksiISO 527-2
Charpy Impact Unnotched 7.00 J/cm²33.3 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 - 225 °C428 - 437 °FDSC; ISO 11357-3
Maximum Service Temperature, Air 210 °C410 °F
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 275 °C482 - 527 °FInjection-molding
Mold Temperature 60.0 - 100 °C140 - 212 °F
 
Descriptive Properties
ColorNatural and Black
Commercial StatusEurope
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® B 4330 G6 HR 30% Glass Filled PBT
BASF Ultradur® B 4300 G6 HR 30% Glass Filled BK 15116 PBT
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT
BASF Ultradur® B 4300 G6 30% Glass Filled PBT
BASF Ultradur® FRee B 4450 G5 LS 25% Glass Filled PBT

PBASG0115 / 131749

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.