MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Clyrell RC 124H Polypropylene
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: The specialty polypropylene Clyrell product portfolio includes random and impact copolymers based on Ziegler-Natta catalysts. Clyrell RC124H is a high modified polypropylene random copolymer designed for extrusion applications.

Clyrell RC124H exhibits enhanced optical properties. The main applications of Clyrell RC124H are blown film extrusion, sheet extrusion and thermoforming. Applications: Bags & Pouches, Food Packaging Film, Stationery Film, Textile Packaging Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 18.0 MPa2610 psiASTM D882
 27.0 MPa
@Thickness 0.0400 mm
3920 psi
@Thickness 0.00157 in
500 mm/min, Blown Film; ASTM D882
Film Tensile Strength at Yield, TD 25.0 MPa
@Thickness 0.0400 mm
3630 psi
@Thickness 0.00157 in
500 mm/min, Blown Film; ASTM D882
Film Elongation at Break, MD 730 %730 %ASTM D 882
 590 %
@Thickness 0.0400 mm
590 %
@Thickness 0.00157 in
500 mm/min, Blown Film; ASTM D 882
Film Elongation at Break, TD 540 %
@Thickness 0.0400 mm
540 %
@Thickness 0.00157 in
500 mm/min, Blown Film; ASTM D 882
Film Elongation at Yield, MD 9.0 %9.0 %500 mm/min, blown film; ASTM 882
Film Elongation at Yield, TD 8.0 %
@Thickness 0.0400 mm
8.0 %
@Thickness 0.00157 in
500 mm/min, blown film; ASTM 882
Secant Modulus, MD 0.840 GPa
@Thickness 0.0400 mm
122 ksi
@Thickness 0.00157 in
23 mm/min, blown film; ASTM D 882
Secant Modulus, TD 0.860 GPa
@Thickness 0.0400 mm
125 ksi
@Thickness 0.00157 in
23 mm/min, blown film; ASTM D 882
Film Tensile Strength at Break, MD 40.0 MPa5800 psiASTM D882
 31.0 MPa
@Thickness 0.0400 mm
4500 psi
@Thickness 0.00157 in
500 mm/min, Blown Film; ASTM D882
Film Tensile Strength at Break, TD 27.0 MPa
@Thickness 0.0400 mm
3920 psi
@Thickness 0.00157 in
500 mm/min, Blown Film; ASTM D882
1% Secant Modulus, MD 600 MPa87000 psiASTM D 882
 
Optical PropertiesMetricEnglishComments
Haze  <= 1.0 %
@Thickness 0.0500 mm
<= 1.0 %
@Thickness 0.00197 in
ASTM D1003
 1.0 %
@Thickness 0.0400 mm
1.0 %
@Thickness 0.00157 in
laboratory blown film; ASTM D1003
Gloss  91 %
@Thickness 0.0500 mm
91 %
@Thickness 0.00197 in
45°; ASTM D 2457
 93 %
@Thickness 0.0400 mm
93 %
@Thickness 0.00157 in
@ 45°, laboratory blown film; ASTM D 2457
 
Descriptive Properties
Processing MethodBlown Film, Sheet, Thermoforming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Clyrell RC 1890 Polypropylene
LyondellBasell Adsyl 5 C 37 F ST Polyolefin
LyondellBasell Adstif HA 3105 Polypropylene
LyondellBasell Clyrell 7173 XCP Polypropylene
LyondellBasell Moplen HP522H Polypropylene

PEQT7090 / 218727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.