MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Clyrell RC 1890 Polypropylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: The specialty polypropylene Clyrell product portfolio includes random and impact copolymers based on Ziegler-Natta catalysts. Clyrell RC1890 is a polypropylene random copolymer; it does not contain slip or anti-block additives and it is Calcium Stearate free. Clyrell RC1890 is designed for the production of blown, oriented and cast film. It is used for a broad range of applications including labels. Applications: Food Packaging Film, Shrink Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 18.0 MPa2610 psiASTM D882
Film Elongation at Break, MD 730 %730 %ASTM D 882
Film Tensile Strength at Break, MD 40.0 MPa5800 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %
@Thickness 0.0500 mm
<= 1.0 %
@Thickness 0.00197 in
Laboratory cast film; ASTM D1003
Gloss 88 %
@Thickness 0.0500 mm
88 %
@Thickness 0.00197 in
@ 45°, laboratory blown film; ASTM D 2457
 
Descriptive Properties
Processing MethodBlown Film, BOPP, Cast Film

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Clyrell RC 124H Polypropylene
LyondellBasell Adsyl 5 C 37 F ST Polyolefin
Equate EGDA-6888 HDPE Film Extrusion Resin

PEQT7089 / 218726

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.