MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zelfo Technology Zelfo® HZ Cellulose Fiber Material
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic

Material Notes: Zelfo® is a high performance bio-based material. Patented fibre technology developed by Zelfo Technology transforms 100% renewable or recycled cellulose fibres and water into self-binding Zelfo material. Zelfo is an economic, adaptable and sustainable alternative to wood, plastics, and other materials for 2D and 3D applications.

Product Design & Built Environment/Construction: Uses across consumer products, packaging, interior design, and construction include housings, furniture, flooring, and paneling. Grade HZ is based on hemp cellulose.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psi
Tensile Modulus 6.55 GPa950 ksi
Flexural Strength 95.0 MPa13800 psi
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²Underground specimens
Izod Impact, Unnotched (ISO) 14.0 kJ/m²6.66 ft-lb/in²Underground specimens

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zelfo Technology Zelfo® HG Cellulose Fiber Material
Telles Mirel™ P1003 Injection Molding Grade PHA Bioplastic
Permabond A1044 Anaerobic Threadsealant
Phillips 66 Cable Lube ISO Grade 15
Wool Cloth Fiber

PZELFO02 / 104604

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.