MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Phillips 66 Cable Lube ISO Grade 15
Categories: Fluid; Lubricant

Material Notes: Cable Lube is a heavy-duty lubricant developed for the lubrication and preservation of wire ropes and cables. It is formulated with a heavy residual base oil and special rust and corrosion inhibitors, and is cut back with a volatile, non-chlorinated solvent for ease of application without heating. Its low viscosity and special wetting properties permit penetration to the core of the wire rope or cable. The solvent evaporates, leaving behind a tough, semifluid lubricant in the core and on each wire strand. Cable Lube clings tenaciously and is not readily displaced by water. It contains an effective rust inhibitor for further protection. Between treatments, lubrication is supplied from the core, which acts as a reservoir to distribute the lubricant to each wire and strand. Cable Lube reduces friction and wear between the wires and strands. The coating on the exterior of the cable protects and lubricates the cable and serves as a cushion between the cable and the sheaves or drums. This residual film remains pliable, even at low ambient temperatures.

Applications:

  • Wire ropes and cables
  • Hoists, cranes, aerial tramways
  • Logging and mining equipment
  • Mill machinery
  • Open and semi-enclosed gears and pinions
  • Guides and sliding surfaces
Features/Benefits:
  • Good penetrating ability
  • Preserves and conditions hemp cores
  • Reduces friction and wear between wires and strands
  • Resists throw-off during high-speed operation
  • Excellent resistance to water washout
  • Excellent rust and corrosion protection

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.883 g/cc0.883 g/cc
Density 0.882 g/cc0.0319 lb/in³
Viscosity Measurement 127127Index, without solvent
Saybolt Viscosity at 100°F 80 SUS80 SUSwith solvent
 7100 SUS7100 SUSwithout solvent
Saybolt Viscosity at 210°F 722 SUS722 SUSwithout solvent
Kinematic Viscosity at 40°C (104°F) 14.5 cSt14.5 cStwith solvent
 1375 cSt1375 cStwithout solvent
Kinematic Viscosity at 100°C (212°F) 150 cSt150 cStwithout solvent
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)ASTM D2596
Four Ball Wear 0.400 mm0.0157 inScar Diameter; ASTM D2266
 
Thermal PropertiesMetricEnglishComments
Pour Point -60.0 °C-76.0 °F
Flash Point 82.0 °C180 °FCOC
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zelfo Technology Zelfo® HZ Cellulose Fiber Material
Zelfo Technology Zelfo® HG Cellulose Fiber Material

WCON5107 / 198360

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.