MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Lustran® SAN 51 Styrene Acrylonitrile (SAN)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Transparent

Material Notes: Lustran® SAN 51 is a transparent styrene acrylonitrile (SAN) with medium flow and highest toughness. Superior chemical and heat resistance, Highest toughness, UL classification 94 HB. Applications: Industrial Battery cases, Disposable lighters, Transparent covers

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D 792
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cmASTM D 955
Melt Flow 6.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 83ASTM D 785
Tensile Strength 75.8 MPaASTM D 638
Tensile Modulus 3380 MPaASTM D 638
Flexural Strength 131 MPaASTM D 790
Flexural Modulus 3590 MPaASTM D 790
Izod Impact, Notched 0.400 ft-lb/in
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched 4.90 ft-lb/in
@Temperature 23.0 °C
ASTM D 256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.0 µin/in-°FASTM D 696
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °Cunannealed; ASTM D 648
 104 °Cannealed; ASTM D 648
Vicat Softening Point 110 °C
@Load 1.02 kg
B/2 120C/H; ASTM D 1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.57Sodium D Line; ASTM D 542
Haze 2.0 %ASTM D 1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 218 - 260 °C
Mold Temperature 38.0 - 82.0 °C
Drying Temperature 82.0 - 88.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 1899 A X 83675 Polycarbonate/Acrylic Alloy (PC/PMMA), Thin Wall Grade
RTP Company RTP 1800 A Z Polycarbonate/Acrylic Alloy (PC/PMMA), FDA Compliant Ingredients
RTP Company RTP 1800 A Polycarbonate/Acrylic Alloy (PC/PMMA), Base Resin
Röhm ACRYLITE® LED LD24 Acrylic Polymer
Lotte Advanced Materials Infino® MR-1020 PC, Medical Grade

PSTYR9834 / 216061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.