MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cossa Polimeri ESTACARB 1601 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Impact Modified

Material Notes: General purpose polycarbonate

High melt flow rate, high impact resistance

Information provided by Cossa Polimeri S.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D 792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D 955
Melt Flow 20 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPaASTM D 638
Tensile Strength, Yield 62.0 MPaASTM D 638
Elongation at Break >= 50 %ASTM D 638
Flexural Modulus 2500 MPaASTM D 790
Izod Impact, Notched 500 J/m
@Temperature 0.000 °C
ASTM D 638
 600 J/m
@Temperature 23.0 °C
ASTM D 256
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 135 °CI.E.C. 335-1
Vicat Softening Point 144 °C
@Load 5.00 kg
50°C/hr; ASTM D 1525
 150 °C
@Load 0.999 kg
50°C/hr; ASTM D 1525
Flammability, UL94 V-2
@Thickness 1.60 mm
 V-2
@Thickness 3.20 mm
Glow Wire Test 850 °C
@Thickness 2.00 mm
I.E.C. 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced
Covestro Apec® HT KU 1-9331 High-Heat Polycarbonate
Lehvoss LUVOCOM® 50/TF/15/BK Polycarbonate with PTFE
Overview of materials for Polycarbonate, Molded

PCOSSA847 / 156437

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.