MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Americas Styrenics Styron® 8100 MFD High Impact Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: STYRON 8100 MFD high impact polystyrene is designed for microfloppy diskettes (MFD) applications. It offers easy processing, coloring, abrasion resistance, impact strength, and high heat resistance. When used unmodified for the manufacture of food contact articles STYRON 8100 MFD complies with the US Food, Drug and Cosmetic Act and Food Additive Regulations 21 CFR 177.1640. The regulations should be consulted for complete details.

Data provided by Dow Chemical.

Americas Styrenics was formed in 2008 as a joint venture between Dow Chemical and Chevron Phillips Chemical Company. Styron was a Dow trade name before the JV formation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM Data
Linear Mold Shrinkage 0.0050 cm/cm
Melt Flow 3.6 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM Data
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105
Tensile Strength, Ultimate 25.0 MPaASTM Data
Tensile Strength, Yield 27.0 MPaASTM Data
Elongation at Break 51 %ASTM Data
Tensile Modulus 2.17 GPaASTM Data
Izod Impact, Notched 1.12 J/cmASTM Data
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 78.0 µm/m-°C
@Temperature 20.0 °C
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °CUnannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °CUnannealed; ASTM Data
Vicat Softening Point 104 °C
Flammability, UL94 HB
@Thickness 3.10 mm
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips EC6600 HIPS - High Impact Polystyrene
Americas Styrenics EB6400 High Impact Polystyrene
Americas Styrenics EA6740 High Impact Polystyrene
Americas Styrenics EC6600 High Impact Polystyrene
Ineos Styrenics Avantra® 585K Q402 Rubber Modified Polystyrene

PDW177 / 34408

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.