MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos Styrenics Avantra® 585K Q402 Rubber Modified Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Avantra® 585K Q402 is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical toughness. Although Avantra® 585K Q402 can be processed by any method applicable to polystyrene-based plastics, it is primarily used for extrusion/thermoforming. Avantra® 585K Q402 has the flow and surface gloss that make it suitable for coextrusion onto HIPS sheet used in durable goods applications like refrigerator liners and point of purchase displays. Unlike GPPS, Avantra® 585K Q402 produces a gloss cap that has excellent toughness with little sacrifice in surface appearance.

Information provided by Ineos Styrenics.


Ineos Styrenics purchased this product line from BASF in 2005.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Water Absorption at Saturation <= 0.10 %<= 0.10 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 3.6 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.6 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 5555ASTM D785
Tensile Strength, Ultimate 24.0 MPa3480 psiASTM D638
Tensile Strength, Yield 26.0 MPa3770 psiASTM D638
Elongation at Break 35 %35 %ASTM D638
Tensile Modulus 2.07 GPa300 ksiASTM D638
Flexural Modulus 1.93 GPa280 ksiASTM D790-1
Izod Impact, Notched 1.23 J/cm2.30 ft-lb/inASTM D256-A
Gardner Impact 28.2 J20.8 ft-lbASTM D5420
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmASTM D257
Dielectric Constant 2.5
@Frequency 100 - 1.00e+6 Hz
2.5
@Frequency 100 - 1.00e+6 Hz
ASTM D150
Dielectric Strength 155 kV/mm3940 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FASTM D648
Vicat Softening Point 101 °C214 °FASTM D1525
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Solid, All Color
 
Optical PropertiesMetricEnglishComments
Gloss 90 %90 %60°; ASTM D523
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 240 °C410 - 464 °FExtrusion
 180 - 280 °C356 - 536 °FMolding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lacqrene® 2901 Medium Impact Polystyrene
Americas Styrenics Styron® 8100 MFD High Impact Polystyrene
Ineos Styrenics Avantra® 2710 High Impact Styrenic Polymer (Global)
Ineos Styrenics Avantra® 585K Rubber Modified Polystyrene
Americas Styrenics EB6400 High Impact Polystyrene

PSF105g / 66686

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.