MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exceed™ m 1018.MF Film Grade Hexene LLDPE
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Exceed™ m 1018 are ethylene 1-hexene copolymer resins. Films made from Exceed™ m 1018 resins have outstanding tensile, impact strength and puncture. These superior strength properties, along with excellent drawability, allow down gauging in bag applications. TnPP is not intentionally added to Exceed™ m 1018 resins

Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America.

Additive: Exceed 1018MF: antiblock: 4500 ppm, slip: 450 ppm; processing aid: yes; thermal stabilizer: yes.

Applications: Agricultural Film; Bag in Box; Barrier Food Packaging; Blown Film; Blown Stretch Film; Bread Bags; Food Packaging; Form Fill And Seal Packaging; Freezer Film; General Packaging; Heavy Duty Bags; Industrial Packaging; Lamination Film; Multilayer Packaging Film; Overwrap Film; Packaging Films; Premium Trash Bags; Stand Up Pouches; Trash Bags; Trash Can Liners

Information provided by ExxonMobil.

Key Words: Exceed™ 1018 MF
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 4500 ppm
Slip Level 450 ppm
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 13.0 lb (f)ExxonMobil Method
Film Tensile Strength at Yield, MD 1300 psiASTM D882
Film Tensile Strength at Yield, TD 1300 psiASTM D882
Film Elongation at Break, MD 500 %ASTM D882
Film Elongation at Break, TD 640 %ASTM D882
Puncture Energy 13.0 in-lbExxonMobil Method
Elmendorf Tear Strength MD 220 gASTM D1922
Elmendorf Tear Strength TD 370 gASTM D1922
Dart Drop Test 550 gASTM D1709A
Film Tensile Strength at Break, MD 9400 psiASTM D882
Film Tensile Strength at Break, TD 8400 psiASTM D882
1% Secant Modulus, MD 24000 psiASTM D882
1% Secant Modulus, TD 26000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 244 °FPeak; ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 16 %ASTM D1003
Gloss 43 %@ 45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2070D Linear Low Density Polyethylene, Blown Film Grade
Dow DOWLEX™ 2045A Linear Low Density Polyethylene, Blown Film Grade
Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade
ExxonMobil Exxtra™ Seal m 1015.MA Film Grade Hexene LLDPE
ExxonMobil Exceed™ m 1018.MJ Film Grade Hexene LLDPE

PEX98850 / 238232

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.