MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: DOWLEX® 2045.02AC Polyethylene resin is a high stability blown film extrusion resin that provides excellent tear strength and outstanding toughness. It contains high level of slip additive and medium level of antiblock additive. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2 (a) for food contact applications, and has been approved by USDA for packaging meat and poultry products.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³
Melt Flow 1.0 g/10 min
@Load 2.16 kg
1.0 g/10 min
@Load 4.76 lb
Melt flow ratio I10/I2 is 8.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 26.2 MPa3800 psiMolded property
Film Tensile Strength at Yield, MD 10.3 MPa1490 psi
Film Tensile Strength at Yield, TD 11.0 MPa1600 psi
Tensile Strength, Yield 12.4 MPa1800 psiMolded property
Film Elongation at Break, MD 650 %650 %
Film Elongation at Break, TD 800 %800 %
Elongation at Break 1000 %1000 %Molded value
Coefficient of Friction 0.200.20
Elmendorf Tear Strength MD 370 g370 gUnspecified film thickness
Elmendorf Tear Strength TD 800 g800 gUnspecified film thickness
Dart Drop Test 250 g0.551 lb
Film Tensile Strength at Break, MD 44.8 MPa6500 psi
Film Tensile Strength at Break, TD 35.2 MPa5110 psi
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 106 °C223 °F
 
Optical PropertiesMetricEnglishComments
Haze 19 %19 %
Gloss 32 %32 %45°
 
Processing PropertiesMetricEnglishComments
Processing Temperature 232 °C450 °FFilm extrusion temperature
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
USDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
Dow DOWLEX™ 2045 Linear Low Density Polyethylene, Heavy Duty Film Grade
Dow DOWLEX™ 2027G Linear Low Density Polyethylene
Dow DOWLEX™ 2025G Linear Low Density Polyethylene

PDW432 / 34501

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.