MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties remain constant after moisture absorption up to a temperature of 60°C [140°F], for instance, for brush collars (electric motors).

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.800 g/cc
Density 1.35 g/ccISO 1183
Moisture Absorption at Equilibrium 1.1 - 1.5 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 5.0 - 6.0 %ISO 62
Viscosity Measurement 130ISO 307
Linear Mold Shrinkage 0.0039 cm/cmrestricted
Linear Mold Shrinkage, Flow 0.0045 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 185 MPa50 mm/min; ISO 527-1/-2
Elongation at Yield 3.0 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 9.00 GPaISO 527-1/-2
Flexural Modulus 7300 MPaISO 178
Izod Impact, Notched (ISO) 8.50 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 80.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Dielectric Constant 4.3
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 33.0 kV/mmIEC 60243-1
Dissipation Factor 0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VTest solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 - 60.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN 11359-1/-2
CTE, linear, Transverse to Flow 25.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN 11359-1/-2
Thermal Conductivity 0.250 W/m-KDIN 52612
Melting Point 295 °CDIN 53765
Maximum Service Temperature, Air 135 °Cfor 50% loss of tensile strength after 20000hr
 160 °Cfor 50% loss of tensile strength after 5000hr
 270 °C
Deflection Temperature at 1.8 MPa (264 psi) 245 °CISO 75-1/-2
Decomposition Temperature >= 350 °C
Flammability, UL94 HB
@Thickness 1.60 mm
Ignition Temperature >= 470 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Zone 1 300 °CFeed Zone
Zone 2 310 °CCompression
Zone 3 320 °CMetering-zone
Zone 4 320 °CNozzle
Melt Temperature 310 - 330 °CInjection-molding/Extrusion
 320 °COptimal
Mold Temperature 80.0 - 120 °CInjection-molding
 100 °COptimal
Drying Temperature 110 °C
Dry Time 8 hour
Moisture Content <= 0.030 %Optimal
 <= 0.15 %
 
Descriptive Properties
ColorBK 00564
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Conditioned)
Evonik VESTAMID® HTplus M1634 PA6T/X, GF30
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry)
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry)
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry)

PBASG0288 / 131921

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.