MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled; Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines flame retardant ability with an excellent balance of high strength, stiffness and heat distortion temperature.

Applications: connectors, terminal blocks, switches and receptacles, coil bobbins, and appliance housing

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.62 g/cc0.0585 lb/in³ASTM D792
Moisture Absorption at Equilibrium 0.90 %0.90 %24 hour; ASTM D570
 1.1 %1.1 %50% RH; ASTM D570
 4.0 %4.0 %Saturation; ASTM D570
Linear Mold Shrinkage 0.00762 cm/cm0.00762 in/in1/8" bar
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121ASTM D785
Tensile Strength at Break 157 MPa22800 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 232 MPa33600 psiASTM D790
Flexural Modulus 8.97 GPa1300 ksiASTM D790
Izod Impact, Notched (ISO) 107 kJ/m²50.9 ft-lb/in²ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmASTM D257
Dielectric Strength 29.0 kV/mm737 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 195 °C383 °FASTM D684
UL RTI, Electrical 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
746B
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0591 in
746B
UL RTI, Mechanical without Impact 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0591 in
746B
Flammability, UL94  V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
 V-0
@Thickness >=2.50 mm
V-0
@Thickness >=0.0984 in
 5VB
@Thickness >=2.50 mm
5VB
@Thickness >=0.0984 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 290 °C482 - 554 °F
Mold Temperature 80.0 - 95.0 °C176 - 203 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content <= 0.15 %<= 0.15 %
 
Descriptive Properties
ColorWhite to gray
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8232G HS FR BK-102 25% Glass Filled PA6 (Dry)
Pasargad Polymer Peyvand Pasamid 3P-H1130W Nylon 6, 30% Glass Fiber Reinforced
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned)
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry)
Envalior Durethan® BKV 30 FN00 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry

PBASG0415 / 132048

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.