MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C19700, H04 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent soldering and brazing. Excellent capacity for both cold and hot forming.

Applications: Electrical and electronic connectors, circuit breaker components, fuse clips, cable shielding, and lead frames. Generally suited to applications requiring excellent formability combined with high strength and conductivity.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7070
Tensile Strength, Ultimate 450 MPa65300 psi
Tensile Strength, Yield 415 MPa60200 psiStrip
Elongation at Break 6.0 %6.0 %In 50 mm
Modulus of Elasticity 121 GPa17500 ksi
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000216 ohm-cm
@Temperature 20.0 °C
0.00000216 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.8 µm/m-°C
@Temperature 20.0 - 100 °C
9.33 µin/in-°F
@Temperature 68.0 - 212 °F
 17.8 µm/m-°C
@Temperature 20.0 - 200 °C
9.89 µin/in-°F
@Temperature 68.0 - 392 °F
 18.3 µm/m-°C
@Temperature 20.0 - 300 °C
10.2 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 320 W/m-K2220 BTU-in/hr-ft²-°F
Melting Point 1069 - 1086 °C1956 - 1987 °F
Solidus 1069 °C1956 °F
Liquidus 1086 °C1987 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 450 - 600 °C842 - 1110 °F
Hot-Working Temperature 750 - 950 °C1380 - 1740 °F
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co <= 0.050 %<= 0.050 %
Copper, Cu 99.15 %99.15 %
Iron, Fe 0.30 - 1.2 %0.30 - 1.2 %
Lead, Pb <= 0.050 %<= 0.050 %
Magnesium, Mg 0.010 - 0.20 %0.010 - 0.20 %
Manganese, Mn <= 0.050 %<= 0.050 %
Phosphorus, P 0.10 - 0.40 %0.10 - 0.40 %
Tin, Sn <= 0.20 %<= 0.20 %
Zinc, Zn <= 0.20 %<= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oxygen-free high conductivity Copper, Hard, UNS C10200
Copper, UNS C19700, H02 Temper
Copper, UNS C18100, Cold Worked (40% reduction) Strip, aged
Copper, UNS C70400, H02 Temper
Oxygen-free high conductivity Copper, Soft, UNS C10200

MC19700b2 / 10975

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.